310 / 1.4841
This material can be supplied as round, heat treated or annealed if desired. It has a very high stainless steel feature due to its austenitic structure. It has a very high resistance to nitrogen and oxygen gases. It has high creep resistance at increasing temperatures. Does not hold magnet.
Especially in high temperature applications, annealing and heat treatment furnaces, heat exchangers, steam boilers, molds operating at high temperatures, glass manufacturing, glass furnaces, rings, grills, thermocouple protective tubes, pipes and cylindrical parts in the petrochemical industry, furnace lids, fans, pipes In short, it is used in almost all areas with high temperature and corrosion wear in its clamps.
DIN X15CrNiSi25-20
1.2782 X16CrNiSi25-20
AFNOR Z10CNS25 20 / Z12CNS25 20
UNI X16CrNiSi25 20
AISI 310 / AISI 314
UNS S31400 / S31000 / S31008
JIS SUH310 / SUH310S
GOST 20Ch25Ni20S2
AISI314
Chemical Composition
C % | Sİ % | Mn % | P % | S % | Cr % | Ni % | N % |
---|---|---|---|---|---|---|---|
≤ 0.20 | ≤ 1.50-2.50 | ≤ 2.00 | ≤ 0.045 | ≤ 0.015 | 24.0-26.0 | 19.0-22.0 | ≤ 0.11 |
Mechanical Properties 20°C
Hardness HB | %0,2 Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation % | Modulus of Elasticity kN/mm² |
---|---|---|---|---|
223 | 230 | 550-750 | 30 | 196 |
Physical Properties 20°C
Density g/cm³ | Specific Heat Capacity J/kg K | Thermal Conductivity W/m K | Electric Resistance Ω mm²/m |
---|---|---|---|
7.9 | 500 | 15 | 0.9 |
AISI310
Chemical Composition
C % | Sİ % | Mn % | P % | S % | Cr % | Ni % | N % |
---|---|---|---|---|---|---|---|
≤ 0.10 | ≤ 1.50 | ≤ 2.00 | ≤ 0.045 | ≤ 0.015 | 24.0-26.0 | 19.0-22.0 | ≤ 0.11 |
Mechanical Properties 20°C
Hardness HB | %0,2 Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation % | Modulus of Elasticity kN/mm² |
---|---|---|---|---|
192 | 210 | 500-700 | 33 | 196 |
Physical Properties 20°C
Density g/cm³ | Specific Heat Capacity J/kg K | Thermal Conductivity W/m K | Electric Resistance Ω mm²/m |
---|---|---|---|
7.9 | 500 | 15 | 0.85 |